Tungsten Processing
2019-8-23 · The tungsten grade is higher than the original ore, grade is 14% to 15%. Extract tungsten from slime is an important method for improving the tungsten recovery rate. Wolframite slime concentration machines have shaker tables, centrifugal concentrators, belt chute, flotation, magnetic separation. The fine mud recovery rate has increased from 10% ...